search  current discussion  categories  kilns & firing - misc 

oxidation or reduction?

updated wed 30 apr 97

 

Steve Williams on tue 29 apr 97

Sorry for the omission folks,
Berry Rust ^7-10 and Pearly ^6 are both oxidation glazes. I haven't tried
either in reduction.

Steve Williams