search  current discussion  categories  kilns & firing - misc 

once fire glaze request

updated fri 31 may 96

 

cape1764@biddeford.com on tue 28 may 96

Howdy all...
I'm having a bit of a hard time finding something that may not seem that
difficult.
I'm looking for a once-fire glaze for ^9-10 Reduction STONEWARE. I would
like it to fire to a clear glossy grey so my slips can show through. I have 2
glazes that work beautifully on raw porcelain but the glaze crawls right off
stoneware. Any suggestions? Any and all would be gratefully appreciated.
TIA Tracy
PS I've got a couple of other interesting glazes. Does anyone out there want to
exchange oncefire glazes?
###############################################
/ / \ Tracy Wilson
/ \ Saltbox Pottery
/ \ RR3 Box 749
/ O | Route 1
/ \ / | Woolwich, Maine 04579
| __V__ | Phone: 207 443-5586
| | | | Fax: 207 443-6544-0
|_________| Email: cape1764@biddeford.com

###############################################