Crystal Larson on tue 9 sep 97
In a message dated 97-09-08 09:59:04 EDT, you write:
<< I think Mishima is a form of decoration achieved by using a very coarse
brush on white slip which has been applied to a coloured body. The brush
marks allow the coloured body to show through the white slip.
I am sure this will lead to a discussion.
>>
that technique is sumi-e where you use the brush stroke to make images.
Mishima is carving first and then brushing the carved area with colored slip
and scraping away the excess to leave a clean line.
Crystal Larson