Corinne Null on sat 12 oct 96

By the way, when I opened the kiln after the super super slow firing
(stalling), there was not one pinhole to be found on the TH blue or Dark
Shiny Blue glazes that I had posted as problems. Hmmmm.

Appreciate all the help, and may still try some of the remedys suggested.

Corinne Null
Bedford, NH

cnull@mv.mv.com