search  current discussion  categories  techniques - moldmaking 

milk mold repair

updated fri 24 oct 97

 

Gaydos, Frank on sun 19 oct 97

John, I cannot imagine how anyone thought to use milk as a glue for
cracked molds. I sh udder at the thought.

Frank in Philly, where it's finally feeling like Fall.

John H. Rodgers on tue 21 oct 97

-- [ From: John H. Rodgers * EMC.Ver #2.5.02 ] --

Frank, that is the wonderful thing about all the good folk who have involved
their lives in clay. They are wonderfully creative, and they experiment,
test, ask questions, brainstorm and share. And the result is sometimes
unusual if not extraordinary. Like realizing the casein in milk would
combine with the calcium in the plaster to make a good bond.

John Rodgers

-------- REPLY, Original message follows --------

Date: Sunday, 19-Oct-97 01:57 PM

From: Gaydos, Frank \ Internet: (fgaydos@ccp.cc.pa.us)
To: CLAYART LIST \ Internet: (clayart@lsv.uky.edu)

Subject: Milk Mold Repair

----------------------------Original message----------------------------
John, I cannot imagine how anyone thought to use milk as a glue for cracked
molds. I sh udder at the thought.

Frank in Philly, where it's finally feeling like Fall.


-------- REPLY, End of original message --------