Frederic Allen Herbst on mon 20 oct 97

I am currently experimenting with salt firing in the range of
cone 4-7. I was wondering if anyone had any interesting glaze, clay or
slip recipes to share. I am particularly interested in fluid glazes
that fire in a wide range (up to cone 9). Anything that can create a
variety of textures (crackles, etc.) would also be great. Thanks for
your help!

Frederic Herbst
UNT Clay
fah0001@jove.acs.unt.edu