Eleanora Eden on tue 10 sep 96

I had a phone call from a friend who has misplaced a glaze and is frantic
for it, unfortunately I was not the person she had given it to.

Desired glaze can be anywhere from cone 6 to cone 10, reduction or
oxydation (tho I think she usually fires cone 10 reduction)

black matte, thick, with irregular surface with pits and craters.
"Like basalt".

I have gone through my clayart files and am sending what I found there,
also the recent tip on adding silicon carbide.

Thanks from us both,

Eleanora

Eleanora Eden 802 869-2003
Paradise Hill
Bellows Falls, VT 05101 eden@maple.sover.net