search  current discussion  categories  tools & equipment - extruders 

lpg needs an extruder

updated fri 31 may 96

 

Gerry Barbe on wed 8 may 96

Hi all,
Marilyn here. The London Potters Guild (in Ontario not the other
London) has been on the hunt for an extruder for three years. The
Northstar is not suitable. What would you recommend for a 70 member
guild? Does anyone between Toronto and Windsor have a good used extruder
for sale?
Thanks, Marilyn Barbe, in training for our clay olympics next Tuesday.
______________________________________________________________________________

LBlos72758@aol.com on fri 10 may 96

Dear Marilyn,

I have the Bailey system extruder. I have a four inch and ten inch box. It
is ten when you count the expansion box. I have it with the pneumatic drive
so that my hands are free to catch the extrusion. It is heavy duty and
requires a small compressor. I would consider it more than adequate for your
setting.

Linda
Ithaca, NY