McCoy, Jack Eugene on thu 30 oct 97

Has anyone had any experience with using fluxes to produce a low-fire,
vitreous clay body?

I have a copy of James Chappels book, which gives a number of recipes
for such bodies. They sound great. But I'd like to see what experience
you have had before I set off to experiment.

Thanks,
Jack McCoy

=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
=-=-=-=-=