search  current discussion  categories  kilns & firing - misc 

kiln lids - too loose

updated sun 31 mar 96

 

Daniel Vito on sun 17 mar 96

Try layer of kiln wash made of 50% alumina hydrate and 50 % kaolin, or
75/25 if you fire to cone 10. The 75/25 mix will remain powdery and can be
brusned off. It won't shrink and can be built up.

Daniel Vito fireborn@lm.com.
Fireborn Studios Ph. (412)488-6835
2338 Sarah Street Fax (412)488-3812
Pittsburgh, PA 15203 "good functional pots"