Lisa on tue 1 oct 96

I'd like to take my favorite ^6 glaze and translate it to ^06 or ^04, but
I don't really know how. Would some of y'all who have recipe software
try this one and see what you come out with? Thanks.

Neph SY 47.3
Gerstley Borate 27.0
Silica 20.3
EPK 5.4

adds: RIO 2%
Cobalt Oxide 1%
Rutile: 4%

TIA from Greensboro, NC