Anne Chambers on wed 23 apr 97

Lisa and everyone else

The Red/Pink Purple/Mauve glaze, as well as the Green Beige glaze that I
posted earlier today are for oxidation. Not for reduction.

When I see ^6 I think oxidation. Lisa, you were asking about a ^6 reduction

Anne Chambers