LINDA BLOSSOM on wed 15 jan 97

I forgot to add. I no longer try to adjust my firing schedule for any
particular glaze. I have a reduction schedule and oxidation schedule. If a
glaze doesn't fit my schedule then out it goes. Bad enough managing both
atmospheres plus the electric kiln. I refuse to baby a glaze anymore. How
many different firings can you put together anyway?



Linda Blossom
2366 Slaterville Rd.
Ithaca, NY 14850
blossom@lightlink.com
http://www.artscape.com
607-539-7912