updated sat 30 nov 96

 

Andrew S Lubow on fri 15 nov 96

They use this glaze a lot at a community college I go to. I'm curious if
anyone can tell me if it's safe used for a food container?

Cone 6 Ed's Plum a lite pink
%
Neph Sy 50.18
Gerstley Borate 8.76
Epk 4.57
Bentonite 0.91
Whiting 21.90
Flint 13.69

Plus:
Tin Oxide 8.21
Potassium Bichromate 0.91


Andy Lubow
Saying Hello 2 JAS@DTE

Andrew S Lubow on tue 19 nov 96

I'm glad to see ClayArt is running again after somebody accidently pulled
the plug last weekend. I'm posting this again since it seems to have been
lost in Cyberspace. If it's a duplicate at your site I apologize.

They use this glaze a lot at a community college I go to. I'm curious if
anyone can tell me if it's safe used for a food container?

Cone 6 Ed's Plum Ox (a lite pink)
%
Neph Sy 50.18
Gerstley Borate 8.76
Epk 4.57
Bentonite 0.91
Whiting 21.90
Flint 13.69

Plus:
Tin Oxide 8.21
Potassium Bichromate 0.91

Andy Lubow
Saying Hello to JAS@DTE

"Live every day like it was your last. Some day you'll be right!!"