search  current discussion  categories  glazes - misc 

crusty glazes

updated fri 28 feb 97

 

JDC on tue 11 feb 97

I guess I've lurked long enough. I am interested in textured glazes for
both raku and cone 10 firing. In raku I've developed some peel off
glazes (mostly clay) as well as "slips" that stay on when fired. I am
interested in knowing if has any hints for me. For cone ten I'm working
on a couple of parched earth shino's (they crack like an AZ riverbed in
June) that I would like to float over some other glaze. I am going to
try Shuges (sp?) black in my next kiln firing. Any suggestions would be
helpful. This list has been a real education. thanks.

Jon Myers
jdc@fta.com