How topical. I posted a recipe incorrectly and illustrated just what you
have all been talking about re: consistant posting.

Here is the correction

Cone 5-6 crackle glaze

Neph Sy .......70
Whiting ........20
Six Tile clay ..10


total 100

Thanks Marcia for bringing it to my attention. The scary thing is....I
proof read it, always do. Oh well, my typing fingers failed me, my eyes
failed me...Sorry for the confusion.

Candice Roeder.