Jennifer Rhinesmith on sat 25 jan 97

HELP!!! I do cone 9-10 reduction firing and there have been some
problems. I have been experimenting with some different glaze recipies
and have had little sucsess. I have been using V.C.'s Wild Wonder and
Ned Coleman's Purple, two glazes that I really love. Everything that I
put them on comes out broken. I mix up my own clay body, for the most
part. Does anyone use these glazes on a basic stoneware body and if so do
you have these problems? I have been told that there is a glaze fit
problem, so can anyone tell me how to remedy this problem. Last semester
I had a 30% loss, and that really hurt. Any info. on this would be
greatly appreciated. Thank You Jennifer in Alpine

Tony Hansen on sun 26 jan 97

Saw you note about crazing on Clayart.
Check the web page at
http://digitalfire.com/magic/archive/crazing.htm
Have a nice day.

--
=================================================================
Tony Hansen, IMC - Get INSIGHT 5 beta or The Magic of Fire II at
http://digitalfire.com or http://www.ceramicsoftware.com