LOWELL BAKER on mon 1 jul 96

We added two cones to see how high we were really firing and found
that we hit cone 12 in ten hours with sawdust. One more firing for
this summer term.

Lowell

tom huber on tue 2 jul 96

Lowell what is your set up for firing with sawdust cone 12 in ten hours is
impressive

thanks tom