Hi All............I remember the time ( about 20 years ago ) when several
comercial companies would mix your own glaze recipe for a fee plus material
costs. I can't locate any now, but would like to. My studio space and
ability to mix up my own glaze is limited. Does anyone know of a company
that will dry mix my recipe ? Much thanks....Romar in Philly

Sue Pellegrini on wed 16 jul 97

Karl Miller used to do it for us years ago. I don't know if Laguna in NY has
continued the practice.

Pelly in Rochester NY

Arturo DeVitalis on thu 17 jul 97

You might try Laguna in Skeaneatales NY, they took over Miller Ceramics
and Carl Miller at one time use to sell large qtys of premixed glazes to
Mike Cohen who was doing a production shop.