broken plaster mold

updated fri 24 oct 97

 

Dana Henson on thu 16 oct 97


Carpenter's wood glue works extremely well. Hope this helps. Dana Henson.
G_Henson@twu.edu

Denis Whitfield on fri 17 oct 97


The white liquid wood working glues are the ones you want. Regardless of
the brand name, they are all PVA (polyvinyl acetate) based - look for
evidence of this on the package.

White liquid adhesive additives for concrete are much the same and are just
as useful - one brand name down under is "Bondcrete".



Denis



At 10:02 16/10/97 EDT, you wrote:
>----------------------------Original message----------------------------
>
>Carpenter's wood glue works extremely well. Hope this helps. Dana Henson.
>G_Henson@twu.edu
>
>
****************************************************************************
DR DENIS WHITFIELD
Senior Lecturer
Coodinator BA(VA)
Co Director, Centre for Ceramic Research, Design and Production
Department of Visual and Peforming Arts
University of Western Sydney, Macarthur
PO Box 555
CAMPBELLTOWN NSW 2560
AUSTRALIA
email: d.whitfield@uws.edu.au
phone: 02 97726345 international: xxx 61 2 97726345
fax: 02 97723244 international: xxx 61 2 97723244
****************************************************************************