Matthew Yanchuk on sat 6 sep 97

What is the procedure for putting handles pulled from lump clay and attaching
them to slip cast cups. Can this be done.

Eleanora Eden on mon 8 sep 97

To Matthew and all,

I have done this with no problems by using solidified slip clay to pull the
handles from. I mean that in the process of removing castings from molds
there's alot of scraps. I take these off before they harden and wedge them
up to use for pulling the handles. Or throwing lids to fit or anything
else you need to add. Works for me.

Eleanora


At 11:12 PM 9/6/97 EDT, you wrote:
>----------------------------Original message----------------------------
>What is the procedure for putting handles pulled from lump clay and attaching
>them to slip cast cups. Can this be done.
>
>
Eleanora Eden 802 869-2003
Paradise Hill
Bellows Falls, VT 05101 eden@sover.net