search  current discussion  categories  forms - tiles 

article on fulper tiles

updated sat 31 aug 96

 

Susan Wagener on wed 7 aug 96

All Martha Stewart jokes aside...there is a good article in the current Martha
Steward Living Magazine September 1996 issue on Fulper Tiles. It's on page 68.

The article discusses how Julia, Anne and Rada Fulper discovered the books
containing their grandfather's glaze formulas in the attic of their childhood
home and have tells the story of how they retested the recipes and started up
their own tile business.

It's a good article...at least I found it interesting since I'm just learning
what goes in to making your own glazes. I can appreciate the work they have
gone to in order to make this business succeed!

Susan Wagener
Puffin Pottery
Bloomington, Indiana where it's hot and steamy!