Robert Speirs, M.D. 12 4450 on tue 17 jun 97

Here's my beautiful glaze. It has a silver overtone that makes it more
interesting than a plain shiny black but it's definitely black and
definitely shiny!

Metallic Black ^5-6

Gerstley Borate ll
Whiting 5
Custer 79
Cobalt OXIDE 2
Copper Carb 4
Manganese Diox. 4

You'll love it.