"s" cracks... throwing pugged clay...

updated mon 31 mar 97

 

Talbott on sun 16 mar 97

Thanks for the valuable info on throwing pugged clay... When are
"S" cracks most likely to occur? (During drying period prior to bisque?)
Why are "S" cracks less likely to form when the log is placed on its side
instead of vertically?

Marshall

1ST ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summmer 1997)
http://fmc.utm.edu/~dmcbeth/cag/naples.htm
>the above site can be viewed but is still under construction<

below are other web-sites which mention the exhibit:
http://www.cclay.com/events.htm
http://www.missouri.edu/~muck/
{contact me directly for more information}

Celia & Marshall Talbott
Pottery By Celia
Route 114
P.O. Box 4116
Naples, Maine 04055-4116
(207)693-6100 voice and fax
clupus@ime.net

Clayarters Live Chat-Room 10:00 pm Eastern Standard Time on Saturday Nites

SHORT CUT if the room has already been created then go to:

http://webchat9.wbs.net/webchat3.so?Room=PRIVATE_Clayarters


or if room has not been created go to WBS at:
http://webchat5.wbs.net/webchat3.so

and set up a "Private Room"... just use the name: Clayarters
------------------------------------------------------------------------------